PosiTector Gage Bodies can be used with all PosiTector probes. Choose from Standard or Advanced models.
PosiTector bodies accept all PosiTector probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, hardness and ultrasonic thickness gage.
Battery-operated and light weight, this Bluetooth Printer prints readings and statistical summaries via Bluetooth from Advanced models.
Verify accuracy/operation of coating thickness gages. Important component of fulfilling both ISO/QS-9000 and in-house quality control requirements with a measurement accuracy traceable to NIST or PTB.
Economical alternative to Coated Metal Plates, with a reduced accuracy. Ideal for protecting the PosiTector probe tip.
Convenient hard shell case for carrying a PosiTector gage body and multiple probes
A lightweight, portable device that allows you to extend the reach of your PosiTector 6000 regular cabled probes.
Use for continuous operation. This kit supplies several alternate power solutions for your battery-operated PosiTector. Operate your gage without the need for batteries.
Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTector instrument.
Every PosiTector 200 and PosiTector UTG ships with (1) bottle of Ultrasonic couplant. Additional 4oz. bottles are available (sold in cases of 12). MSDS
Genuine leather pouch protects your PosiTest DFT while keeping it within easy reach.
Pack of 5 thin plastic lens shields to protect PosiTector display from paint overspray. One lens shield included in every PosiTector purchase.
Ideal for applications where the USB cable will stay connected to the PosiTest PC while taking measurements.
Provide a quick operational check of the instrument by allowing the user to perform practice measurements
Helps reduce adverse operator influence by ensuring the PosiTector 6000 probe is placed perpendicular to the part’s surface in a controlled, repeatable way.
Ideal for use on thin, soft coatings to protect coatings from unnecessary wear while using Scan or Fast mode to measure large objects
Used to protect the PosiTest PC probe transducer (Qty. 2)
Certified Polystyrene Blocks are for use with gages that measure over 1500 µm (60 mils).
PosiTector Gage Bodies can be used with all PosiTector probes. Choose from Standard or Advanced models.
PosiTector bodies accept all PosiTector probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, hardness and ultrasonic thickness gage.
Battery-operated and light weight, this Bluetooth Printer prints readings and statistical summaries via Bluetooth from Advanced models.
Round-end plastic rubbing tool to compress replica film on the blasted surface (Pack of 10)
Convenient hard shell case for carrying a PosiTector gage body and multiple probes
Each roll of Testex Tape includes 50 pieces (Impressions)
Use for continuous operation. This kit supplies several alternate power solutions for your battery-operated PosiTector. Operate your gage without the need for batteries.
Used to verify the accuracy and operation of all Testex micrometers. Ideal for fulfilling both ISO and in-house quality control requirements. Includes Certificate of Calibration traceable to PTB.
Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTector instrument.
For best results when acquiring a 2D/3D parameters and images, it is recommended to use the supplied burnishing ball instead of the stainless-steel burnishing tool.
Used to check PosiTector RTR peak height accuracy (RTR H and RTR 3D). One check shim is included with each probe.
For best results and to minimize the migration of adhesive from the tape to the probes measurement system, DeFelsko recommends using the supplied tape holder.
To clean the test surface of debris prior to burnishing
Pre-moistened with isopropyl alcohol to clean residual adhesive and debris from the PosiTector RTR and RTR 3D anvils helping to ensure an accurate test.
Used to verify the accuracy and operation of Testex and other spring micrometer replica tape readers
Burnishing tool includes a built-in spring mechanism ensuring that consistent force is used, regardless of how hard the tool is pressed against the surface
Provides a quick accuracy check of the PosiTector SPG and allows the user to perform practice measurements
Pack of 5 thin plastic lens shields to protect PosiTector display from paint overspray. One lens shield included in every PosiTector purchase.
For enhanced stability on 30 - 45 cm (12 - 18") OD pipes (for PosiTector SPG OS only).
Replacement probe tips for the PosiTector SPG — 2 angles available: 60° or 30°
Used to check the operation of PosiTector RTR 3D peak density measurement (for use with the PosiTector RTR 3D only).
Used to verify the accuracy and operation of surface profile depth micrometers
Contains a pattern with a known peak-to-valley profile height, to learn and verify correct measurement technique
PosiTector Gage Bodies can be used with all PosiTector probes. Choose from Standard or Advanced models.
PosiTector bodies accept all PosiTector probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, hardness and ultrasonic thickness gage.
Dew Point Meter Logger attaches to steel structures to measure and record environmental parameters independently for up to 200 days.
Battery-operated and light weight, this Bluetooth Printer prints readings and statistical summaries via Bluetooth from Advanced models.
Convenient hard shell case for carrying a PosiTector gage body and multiple probes
Use for continuous operation. This kit supplies several alternate power solutions for your battery-operated PosiTector. Operate your gage without the need for batteries.
Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTector instrument.
Pack of 5 thin plastic lens shields to protect PosiTector display from paint overspray. One lens shield included in every PosiTector purchase.
Hand-held Surface Temperature Probe and Liquid Temperature Probe. For use with PosiTector DPMS probes only.
Optional Lock keeps the PosiTector DPM L safe and secure
Available in packs of five (5) CR2032 batteries for use with the PosiTector DPM L.
10 pack of replacement filters for the PosiTector DPM L
Reusable Bresle Test patch with Standard or Flexible magnetic ring for soluble salt testing
Latex Bresle Test patch with easy-open tabs and low-tack adhesive for easy removal for soluble salt testing
Self-adhesive, polyurethane Bresle Test patches for soluble salt testing
PosiTector Gage Bodies can be used with all PosiTector probes. Choose from Standard or Advanced models.
PosiTector bodies accept all PosiTector probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, hardness and ultrasonic thickness gage.
Battery-operated and light weight, this Bluetooth Printer prints readings and statistical summaries via Bluetooth from Advanced models.
For use with existing conductivity meters. Try the revolutionary, reusable Bresle Method PosiPatch with a low cost trial pack.
Measures the concentration of water-soluble contaminates in blast cleaning abrasives
Like the Standard Magnetic Ring PosiPatch, the NEW Flexible Magnetic ring leaves no messy adhesive residue to clean but is intended for pipes and other tight-diameters.
Use for continuous operation. This kit supplies several alternate power solutions for your battery-operated PosiTector. Operate your gage without the need for batteries.
Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTector instrument.
Purified, ion-free water to be used with the PosiTector SST, 250 ml or 1 l
To verify accuracy of PosiTector SST probe
Pack of 5 thin plastic lens shields to protect PosiTector display from paint overspray. One lens shield included in every PosiTector purchase.
100 pack - 125 mm for use with PosiTector SST Abrasives Test Kit
Plastic dispensing tips for the PosiTector SST (10 pack)
Replacement dust tape comparator, transparent display board, and (4) 25 pack of Report Forms
(1) Roll of ISO 8502-3 Tape for use with PosiTest DT test—25 mm wide
Additional glue, mixing sticks, palettes and cotton swabs for pull-off adhesion tests
Drilling template and drill bits to isolate test area for pull-off adhesion tests, ideal for thicker coatings on concrete.
Interchangeable stand-off allows a PosiTest ATM50 or ATA50 to pull 10, 14 and 20 mm dollies. Ideal for high bond strength finishes such as coatings on metal.
Interchangeable stand-off allows a PosiTest ATM20 or ATA20 to pull 50 mm dollies. Ideal for lower bond strength finishes such as coatings on wood, concrete and plastic.
Interchangeable stand-off allows a PosiTest ATM or ATA to pull 50 mm x 50 mm square dollies conforming to BS EN 12004-2. Ideal for cementitious adhesive for tiles.
Interchangeable stand-off allows a PosiTest ATM or ATA to pull 50 mm dollies conforming to ASTM C1583. Ideal for concrete surfaces and overlays.
Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTest instrument.
Ideal for checking the accuracy and operation of PosiTest Adhesion Testers and is an important component in fulfilling both ISO and in-house quality control requirements.
Roll of replacement tape for PosiTest CH Cross Hatch Adhesion Test
(1) Roll of ISO 8502-3 Tape for use with PosiTest DT test—25 mm wide
4-in-1 Replacement Blades for PosiTest CH Cross Hatch Tool
Add additional, reusable PosiTector CMM IS Smart probes
A 10-pack of the Salt Solution for use with the PosiTector CMM IS
Replacement caps for use with the PosiTector CMM IS
Available in packs of ten A-76/LR-44 coin cell batteries for use with the PosiTector CMM IS.
Replacement fins for the PosiTector CMM IS
Replacement extraction tool for use with the PosiTector CMM IS.
Available in packs of 3.
For extending PosiTector CMM IS probe height in concrete slab thicknesses deeper than 4 inches
This lightweight device increases the utility of the PosiTest CMM allowing for quick and easy concrete moisture measurements on large surfaces without the need to bend or kneel.
PosiTector Gage Bodies can be used with all PosiTector probes. Choose from Standard or Advanced models.
PosiTector bodies accept all PosiTector probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, hardness and ultrasonic thickness gage.
Battery-operated and light weight, this Bluetooth Printer prints readings and statistical summaries via Bluetooth from Advanced models.
Ideal for checking calibration and operation of ultrasonic thickness gages and are an important component in fulfilling both ISO and in-house quality control requirements.
Convenient hard shell case for carrying a PosiTector gage body and multiple probes
Use for continuous operation. This kit supplies several alternate power solutions for your battery-operated PosiTector. Operate your gage without the need for batteries.
Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTector instrument.
Every PosiTector 200 and PosiTector UTG ships with (1) bottle of Ultrasonic couplant. Additional 4oz. bottles are available (sold in cases of 12). MSDS
Pack of 5 thin plastic lens shields to protect PosiTector display from paint overspray. One lens shield included in every PosiTector purchase.
PosiTector Gage Bodies can be used with all PosiTector probes. Choose from Standard or Advanced models.
PosiTector bodies accept all PosiTector probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, hardness and ultrasonic thickness gage.
Battery-operated and light weight, this Bluetooth Printer prints readings and statistical summaries via Bluetooth from Advanced models.
Convenient hard shell case for carrying a PosiTector gage body and multiple probes
Use for continuous operation. This kit supplies several alternate power solutions for your battery-operated PosiTector. Operate your gage without the need for batteries.
Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTector instrument.
Ideal for checking the operation of durometers.
Helps reduce operator influence by ensuring the probe is placed perpendicular in a controlled, repeatable way.
For use with threaded mounts in other test stands and calibrators.
Pack of 5 thin plastic lens shields to protect PosiTector display from paint overspray. One lens shield included in every PosiTector purchase.
For zeroing worn or replaced indentors on the PosiTector BHI.
For verifying the operation of Barcol hardness impressors. Choose from hard, soft, or extra soft aluminum alloys. (Pack of 5)
Includes additional spare indentor tips (2pk) with replacement tool for the PosiTector BHI.
Available as a complete set of 14 or as a 12 pack for individual hardnesses
Replacement Blades (qty 10) for PosiTest PT Pencil Sharpener
For visual assessment of scratch and gouge marks
Shoulder strap for the PosiTest HHD Basic Kit
Replacement Li-ion batteries for the PosiTest HHD series
Converts the PosiTest HHD to a wand-type instrument
Thread onto rolling springs and attach to the Spring Connector for the PosiTest HHD series
102mm/4" Conductive Rubber Paddle for PosiTest HHD
Adaptable Sponge Hardware for a variety of test configurations with the PosiTest LPD
43 cm (17") Extension Rod for PosiTest HHD C
Converts the PosiTest LPD Low voltage Pinhole Detector into a cabled-wand style unit.
Connect the PosiTest HHD to DeFelsko or SPY rolling spring electrodes
Choose between 13 cm (5") and 50 cm (20") rods for PosiTest HHD
For verification of electrical resistance
Stainless steel fan brush for PosiTest HHD series — 152 mm (6”)
Pinholes can be so miniscule that water has difficulty reaching the conductive substrate underneath. Use a surfactant (wetting agent) to lower the surface tension of the water.
Connect to spring and brush electrodes to PosiTest HHD from other manufacturers
Extend the PosiTest LPD base rod an additional 0.3 m (1')
Standalone voltmeter (crest meter, jeep meter) for verifying the accuracy and operation of pulse or continuous type DC holiday detectors
Neoprene half-circle brush electrode for PosiTest HHD series—good for pipes 50 to 127 mm / 2 to 5 inches
Steel pipe electrodes for PosiTest HHD series — assorted sizes available: 10 to 91 cm (4 – 36”) Rolling springs include two pre-installed spring couplers.
610 mm (24") roller sponge for quick inspection over large areas with the PosiTest LPD
Stainless steel flat wire brush electrodes for PosiTest HHD series — assorted sizes available: 5 to 120 cm (2 – 48”)
Includes adaptable sponge hardware and accessories to convert the PosiTest LPD Basic Kit into a PosiTest LPD Complete Kit.
PosiTector Gage Bodies can be used with all PosiTector probes. Choose from Standard or Advanced models.
PosiTector bodies accept all PosiTector probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, hardness and ultrasonic thickness gage.
Battery-operated and light weight, this Bluetooth Printer prints readings and statistical summaries via Bluetooth from Advanced models.
Use for continuous operation. This kit supplies several alternate power solutions for your battery-operated PosiTector. Operate your gage without the need for batteries.
Pack of 5 thin plastic lens shields to protect PosiTector display from paint overspray. One lens shield included in every PosiTector purchase.
10 pack of replacement cleaning wipes for the PosiTector GLS
A wide variety of temperature probes are available for the PosiTest OTL with 1.8, 3.6, or 6 m (6', 12', or 20') stainless steel braided cables (sold separately).
Six (6) replacement engraved ID tags for PosiTest OTL temperature probes
Reusable Bresle Test patch with Standard or Flexible magnetic ring for soluble salt testing
Latex Bresle Test patch with easy-open tabs and low-tack adhesive for easy removal for soluble salt testing
Self-adhesive, polyurethane Bresle Test patches for soluble salt testing
PosiTector Gage Bodies can be used with all PosiTector probes. Choose from Standard or Advanced models.
PosiTector bodies accept all PosiTector probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, hardness and ultrasonic thickness gage.
Dew Point Meter Logger attaches to steel structures to measure and record environmental parameters independently for up to 200 days.
Battery-operated and light weight, this Bluetooth Printer prints readings and statistical summaries via Bluetooth from Advanced models.
Round-end plastic rubbing tool to compress replica film on the blasted surface (Pack of 10)
Ideal for checking calibration and operation of ultrasonic thickness gages and are an important component in fulfilling both ISO and in-house quality control requirements.
For use with existing conductivity meters. Try the revolutionary, reusable Bresle Method PosiPatch with a low cost trial pack.
Verify accuracy/operation of coating thickness gages. Important component of fulfilling both ISO/QS-9000 and in-house quality control requirements with a measurement accuracy traceable to NIST or PTB.
Measures the concentration of water-soluble contaminates in blast cleaning abrasives
Like the Standard Magnetic Ring PosiPatch, the NEW Flexible Magnetic ring leaves no messy adhesive residue to clean but is intended for pipes and other tight-diameters.
Economical alternative to Coated Metal Plates, with a reduced accuracy. Ideal for protecting the PosiTector probe tip.
Convenient hard shell case for carrying a PosiTector gage body and multiple probes
Each roll of Testex Tape includes 50 pieces (Impressions)
A lightweight, portable device that allows you to extend the reach of your PosiTector 6000 regular cabled probes.
Use for continuous operation. This kit supplies several alternate power solutions for your battery-operated PosiTector. Operate your gage without the need for batteries.
Used to verify the accuracy and operation of all Testex micrometers. Ideal for fulfilling both ISO and in-house quality control requirements. Includes Certificate of Calibration traceable to PTB.
Additional glue, mixing sticks, palettes and cotton swabs for pull-off adhesion tests
Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTector instrument.
Purified, ion-free water to be used with the PosiTector SST, 250 ml or 1 l
Every PosiTector 200 and PosiTector UTG ships with (1) bottle of Ultrasonic couplant. Additional 4oz. bottles are available (sold in cases of 12). MSDS
To verify accuracy of PosiTector SST probe
Drilling template and drill bits to isolate test area for pull-off adhesion tests, ideal for thicker coatings on concrete.
Shoulder strap for the PosiTest HHD Basic Kit
Replacement Li-ion batteries for the PosiTest HHD series
Interchangeable stand-off allows a PosiTest ATM50 or ATA50 to pull 10, 14 and 20 mm dollies. Ideal for high bond strength finishes such as coatings on metal.
Interchangeable stand-off allows a PosiTest ATM20 or ATA20 to pull 50 mm dollies. Ideal for lower bond strength finishes such as coatings on wood, concrete and plastic.
Converts the PosiTest HHD to a wand-type instrument
Thread onto rolling springs and attach to the Spring Connector for the PosiTest HHD series
102mm/4" Conductive Rubber Paddle for PosiTest HHD
Interchangeable stand-off allows a PosiTest ATM or ATA to pull 50 mm x 50 mm square dollies conforming to BS EN 12004-2. Ideal for cementitious adhesive for tiles.
Interchangeable stand-off allows a PosiTest ATM or ATA to pull 50 mm dollies conforming to ASTM C1583. Ideal for concrete surfaces and overlays.
Adaptable Sponge Hardware for a variety of test configurations with the PosiTest LPD
For best results when acquiring a 2D/3D parameters and images, it is recommended to use the supplied burnishing ball instead of the stainless-steel burnishing tool.
43 cm (17") Extension Rod for PosiTest HHD C
Converts the PosiTest LPD Low voltage Pinhole Detector into a cabled-wand style unit.
Connect the PosiTest HHD to DeFelsko or SPY rolling spring electrodes
Used to check PosiTector RTR peak height accuracy (RTR H and RTR 3D). One check shim is included with each probe.
Choose between 13 cm (5") and 50 cm (20") rods for PosiTest HHD
For verification of electrical resistance
Stainless steel fan brush for PosiTest HHD series — 152 mm (6”)
For best results and to minimize the migration of adhesive from the tape to the probes measurement system, DeFelsko recommends using the supplied tape holder.
To clean the test surface of debris prior to burnishing
Pinholes can be so miniscule that water has difficulty reaching the conductive substrate underneath. Use a surfactant (wetting agent) to lower the surface tension of the water.
Ideal for checking the operation of durometers.
Connect to spring and brush electrodes to PosiTest HHD from other manufacturers
Extend the PosiTest LPD base rod an additional 0.3 m (1')
Pre-moistened with isopropyl alcohol to clean residual adhesive and debris from the PosiTector RTR and RTR 3D anvils helping to ensure an accurate test.
Standalone voltmeter (crest meter, jeep meter) for verifying the accuracy and operation of pulse or continuous type DC holiday detectors
Helps reduce operator influence by ensuring the probe is placed perpendicular in a controlled, repeatable way.
Used to verify the accuracy and operation of Testex and other spring micrometer replica tape readers
Neoprene half-circle brush electrode for PosiTest HHD series—good for pipes 50 to 127 mm / 2 to 5 inches
For use with threaded mounts in other test stands and calibrators.
Steel pipe electrodes for PosiTest HHD series — assorted sizes available: 10 to 91 cm (4 – 36”) Rolling springs include two pre-installed spring couplers.
Heavy-duty, waterproof Pelican cases complete with a custom foam insert to securely hold your PosiTest instrument.
610 mm (24") roller sponge for quick inspection over large areas with the PosiTest LPD
Ideal for checking the accuracy and operation of PosiTest Adhesion Testers and is an important component in fulfilling both ISO and in-house quality control requirements.
Stainless steel flat wire brush electrodes for PosiTest HHD series — assorted sizes available: 5 to 120 cm (2 – 48”)
Includes adaptable sponge hardware and accessories to convert the PosiTest LPD Basic Kit into a PosiTest LPD Complete Kit.
Add additional, reusable PosiTector CMM IS Smart probes
Burnishing tool includes a built-in spring mechanism ensuring that consistent force is used, regardless of how hard the tool is pressed against the surface
Genuine leather pouch protects your PosiTest DFT while keeping it within easy reach.
Provides a quick accuracy check of the PosiTector SPG and allows the user to perform practice measurements
Pack of 5 thin plastic lens shields to protect PosiTector display from paint overspray. One lens shield included in every PosiTector purchase.
Ideal for applications where the USB cable will stay connected to the PosiTest PC while taking measurements.
Provide a quick operational check of the instrument by allowing the user to perform practice measurements
For zeroing worn or replaced indentors on the PosiTector BHI.
For enhanced stability on 30 - 45 cm (12 - 18") OD pipes (for PosiTector SPG OS only).
A 10-pack of the Salt Solution for use with the PosiTector CMM IS
Replacement probe tips for the PosiTector SPG — 2 angles available: 60° or 30°
For verifying the operation of Barcol hardness impressors. Choose from hard, soft, or extra soft aluminum alloys. (Pack of 5)
Helps reduce adverse operator influence by ensuring the PosiTector 6000 probe is placed perpendicular to the part’s surface in a controlled, repeatable way.
Ideal for use on thin, soft coatings to protect coatings from unnecessary wear while using Scan or Fast mode to measure large objects
Replacement caps for use with the PosiTector CMM IS
100 pack - 125 mm for use with PosiTector SST Abrasives Test Kit
Every PosiTest AIR comes complete with (4) bottles of Test Solution. Additional bottles are available in cases of (16) 8 oz. bottles.
Used to protect the PosiTest PC probe transducer (Qty. 2)
Certified Polystyrene Blocks are for use with gages that measure over 1500 µm (60 mils).
Used to check the operation of PosiTector RTR 3D peak density measurement (for use with the PosiTector RTR 3D only).
Available in packs of ten A-76/LR-44 coin cell batteries for use with the PosiTector CMM IS.
Replacement fins for the PosiTector CMM IS
Includes additional spare indentor tips (2pk) with replacement tool for the PosiTector BHI.
Hand-held Surface Temperature Probe and Liquid Temperature Probe. For use with PosiTector DPMS probes only.
Used to verify the accuracy and operation of surface profile depth micrometers
Replacement extraction tool for use with the PosiTector CMM IS.
Available in packs of 3.
For extending PosiTector CMM IS probe height in concrete slab thicknesses deeper than 4 inches
Optional Lock keeps the PosiTector DPM L safe and secure
Available in packs of five (5) CR2032 batteries for use with the PosiTector DPM L.
A wide variety of temperature probes are available for the PosiTest OTL with 1.8, 3.6, or 6 m (6', 12', or 20') stainless steel braided cables (sold separately).
Six (6) replacement engraved ID tags for PosiTest OTL temperature probes
This lightweight device increases the utility of the PosiTest CMM allowing for quick and easy concrete moisture measurements on large surfaces without the need to bend or kneel.
Plastic dispensing tips for the PosiTector SST (10 pack)
10 pack of replacement cleaning wipes for the PosiTector GLS
10 pack of replacement filters for the PosiTector DPM L
Contains a pattern with a known peak-to-valley profile height, to learn and verify correct measurement technique
Roll of replacement tape for PosiTest CH Cross Hatch Adhesion Test