Testex Micrometer Kits include everything required to measure surface profile using replica tape
Features:
Guide and visual reference photographs to supplement SSPC/NACE written standards.
Notched Wet Film Thickness Gages measure the thickness of paint, enamels, and other wet films quickly and accurately
Features:
Determines a coating’s ability to resist separation from a substrate when a lattice pattern is cut into the coating in accordance with ISO 2409 and ASTM D3359
Features
Assesses the quantity and size of dust particles on blast cleaned surfaces in accordance with ISO 8502-3
Features
Determines the film hardness by pencil test (Wolff-Wilborn) in accordance with national and international standards including ISO 15184 and ASTM D3363
Features:
DeFelsko is pleased to announce the newest addition to the PosiTest line of pinhole and porosity detectors—the PosiTest HHD C High voltage Holiday Detector. The NEW compact, wand-style PosiTest HHD C uses continuous DC technology to detect holidays in coatings greater than 200 µm (8 mils) on metal and concrete substrates.
Features:
The new PosiTector GLS Gloss Meter brings Gloss, Reflectances, and Haze measurement to the PosiTector platform. Select up to three measurement angles to suit any application, save readings into memory, and transfer them to PosiSoft Software to quickly archive data and generate professional reports. The PosiTector GLS brings DeFelsko simplicity, durability, and accuracy to gloss measurement.
Features:
Featuring near-instant readings and no requirement to drill into the concrete, the PosiTest CMM is ideal for inspectors looking to quickly evaluate the moisture conditions in concrete slabs. It joins the DeFelsko line of concrete moisture measurement equipment alongside the highly-accurate PosiTector CMM IS In-situ Concrete Moisture Meter.
Features:
The new PosiTest HHD Basic Kit includes the same award-winning PosiTest HHD High voltage Holiday Detector in a more economical kit configuration. This new kit reduces weight and shipping costs while keeping the durability and versatility of the original, offering compatibility with all PosiTest HHD electrodes and accessories including the Handheld Wand.
New Features:
The PosiTest AT-M Manual Adhesion Tester has been updated with a new high-contrast, easy-to-read color display, a redesigned keypad, and field replaceable AAA alkaline batteries which provide up to 16 hours of testing. For easy setup and confirmation, the updated user interface shows important pull parameters before, during, and after the test.
New Features:
Featuring compatibility with all PosiTector probes manufactured since 2012, the new PosiTector gage body builds on this legacy with many industry leading new features.
New Features:
DeFelsko is pleased to announce the new PosiTest OTL Oven Temperature Logger. Featuring a high temperature stainless steel barrier box, the PosiTest OTL is ideal for measuring and recording oven temperature profiles during curing. Simultaneously measure up to 6 different temperatures at a time with a variety of air and surface temperature probes (sold separately).
Features:
Depending on time and temperature requirements, the PosiTest OTL is available in two configurations. The PosiTest OTL XT features an enhanced holder with heatsink for greater endurance at high temperatures.
A wide variety of temperature probes are available with 1.8 or 3.6 m (6' or 12') stainless steel braided cables (sold separately).
The new PosiTector DPM L Dew Point Meter Logger magnetically attaches to steel structures to measure and record climatic conditions at user-selected time intervals independently for up to 200 days. Stored datasets can be viewed or downloaded using a PosiTector Advanced gage body (S/N 784000+) or Apple/Android smart device.
At each interval, the PosiTector DPM L stores relative humidity, air temperature, surface temperature, dew point temperature, the difference between surface and dew point temperatures, and wet bulb temperature. Ideal for surface preparation as required by ISO 8502-4.
Features:
DeFelsko is pleased to announce the updated PosiTector RTR H Replica Tape Reader probe, a digital spring micrometer that measures peak-to-valley surface profile height using Testex Press-O-Film Replica Tape. The new probe has been redesigned to include a wider opening for easier tape placement.
The rugged PosiTector RTR H offers many improvements over conventional micrometers.
*With a single measurement, the PosiTector RTR H produces a linearized peak-to-valley height measurement (HL), accurate over the full range of Coarse and X-Coarse tapes. There is no need to average two or more replicas to ensure accuracy.
PosiTector 6000 gages now feature a new Prompted Batch Mode to simplify inspections. Create pre-defined batches in PosiSoft Desktop with onscreen text and image prompts for each reading, then upload to PosiTector 6000 gages (Advanced models, serial numbers 784000 only).
To start using Prompted Batch Mode, download the latest version of PosiSoft Desktop from our website. A simple gage update adds this functionality to existing PosiTector 6000Advanced models (serial numbers 784000 and greater).
DeFelsko is pleased to introduce the new PosiTest LPD Cabled Wand. This new accessory converts the PosiTest LPD Low voltage Pinhole Detector into a cabled wand-style unit. At just 13.5 cm (5.3”), it is ideal for ergonomically measuring hard-to-reach areas.
Includes a remote wand handle and 1.5 m (5’) hot wire cable. The wand handle is compatible with the rectangular and roller sponge hardware from the PosiTest LPD Basic and/or Complete Kits (not included).
A precision step block is now available for verifying the accuracy and operation of the PosiTector UTG P Precision Ultrasonic Wall Thickness Gage.
Material: 1018 Steel
Step Height: 40, 60, 80, and 100 mils (metric equivalent: 1, 1.5, 2, and 2.5 mm - labeled in imperial units only)
Introducing the new PosiTector 6000 FJS Coating Thickness probe for measuring thick, protective coatings on steel. With a measurement range of 0 to 25 mm (0 to 1.00 in.), It is ideal for measuring thick epoxies, rubbers, fireproofing, and other thick coatings applied to steel.
Compared to the higher range PosiTector 6000 FLS, this new probe features an alumina wear face and a lightweight, ergonomic design for comfortable all-day use. In fact, the new PosiTector 6000 FJS probe is about 66% smaller than comparable probes. Unlike competitive probes based on eddy-current technology, the electro-magnetic technology in PosiTector 6000 probes (including the PosiTector 6000 FJS) is less susceptible to the effects of substrate roughness, curvature, material, and alloy.
Introducing the PosiTector UTG CA, UTG CLF, and UTG P
DeFelsko is excited to announce a new probe for the PosiTector SPG Surface Profile Gage. The PosiTector SPG OS probe is ideal for measuring the peak-to-valley surface profile height of convex abrasive blast cleaned surfaces such as pipes and tanks.
Features
DeFelsko is excited to announce the addition of WiFi Streaming and Bluetooth Low Energy features to the PosiTector Developer Resources. These resources allow app developers to integrate with third-party software using several industry-standard communication protocols.
From wired USB to WiFi wireless technology, DeFelsko offers data management solutions for even the most advanced software integrations with drones, ROVs, PLCs and more. Accessing your stored or live streaming data is simpler and more flexible than ever before.
DeFelsko is excited to announce that the new PosiTest HHD High voltage Holiday Detector is now shipping. The PosiTest HHD uses pulse DC technology, offering a user-adjustable voltage range from 0.5 to 35kV for detecting holidays, pinholes and other discontinuities in coatings up to 20 mm (780 mils) thick.
The versatile PosiTest HHD is ideal for use with a wide range of rolling spring and flat wire brush electrodes — custom sizes are available upon request. Alternatively, use existing electrodes with industry-standard adaptors.
Key Features
Introducing the newly redesigned PosiTector 6000 FXS Xtreme Coating Thickness probe – built for hot surfaces and rugged applications including hot dipped and thermally sprayed galvanizing on steel. This updated probe features an improved zirconia-toughened alumina wear face and a new braided stainless steel cable making it ideal for harsh conditions and continuous measurement on hot substrates up to 250˚ C (500˚ F).
The PosiTector 6000 FXS Xtreme probe now features an increased range of 0 – 2000 µm (80 mil).
Features
DeFelsko is excited to announce two new zero plate sizes for use with PosiTector 6000 probes. Now available in small, medium and large sizes with steel and aluminum (6061-T6) options.
The new larger Zero Plates feature precision machined metal with an increased surface area and thickness. They are ideal for use when verifying the accuracy or operation of PosiTector 6000 thick probes using Certified Polystyrene blocks and shims.
The new PosiTest PC Powder Checker measures uncured powder coatings using non-contact ultrasound technology to predict a cured thickness. The instrument has been completely redesigned as a dedicated stand-alone unit -- no PosiTector gage body required. With a measurement speed up to 4x faster than previous models the new PosiTest PC is easier to use, especially on moving parts and challenging geometries.
Features
* Versus the previous generation PosiTector PC Powder Checker
The new PosiTector UTG CX Xtreme corrosion probe features the same trusted and precise ultrasonic technology as the PosiTector UTG Cprobe but with the addition of a robust braided stainless steel cable. It is the direct result of inspectors’ requests for a probe that features the same accuracy and ease-of-use of the current PosiTector UTG C but with the ruggedness to handle demanding applications.
Features
The PosiTector 200 is the result of five generations of product innovation, and for many applications, remains the only economical solution for measuring coating thickness on wood, plastic, concrete and more. This ‘one of a kind’ instrument provides distributors with the unique opportunity to sell a product with significant market potential.
The PosiTector 200’s ultrasonic technology is as simple to use as the PosiTector 6000, but some distributors and customers are reluctant to use an instrument that operates differently than conventional DFT gages for steel. For those unfamiliar with the easy-to-use PosiTector200, watch DeFelsko’s new video showcasing the key features and simple operation.
Click the link below to watch the video overview on the PosiTector 200 - the history and its proven ultrasonic technology.
The new PosiTector BHI Barcol Hardness Impressor is DeFelsko’s latest addition to the PosiTector line of interchangeable probes. It is ideal for measuring the indentation hardness of soft metals (aluminum, aluminum alloys, copper, brass, etc.), harder plastics and fiber-reinforced plastics.
Features
The new Large Pelican™ Inspection Case offers rugged protection for larger PosiTector® inspection kits. Each case securely stores a PosiTector gage body and 5+ PosiTector probes. The center insert is ideal for PosiTector SST Soluble Salt Tester accessories and can be removed to store more inspection equipment and accessories.
Features
The new PosiTector IRT non-contact Infrared Thermometer measures surface temperature from a distance - ideal for areas where conventional sensors will not work including hard to reach areas and moving parts. It is also ideal for measuring on objects too hot for direct contact sensors or when contact with a sensor would damage the surface.
Features
PosiTrack is an online portal offering free gage management tools to print Certificates of Calibration, set email calibration reminders and access service forms. The interface displays a list of equipment with serial numbers alongside calibration and in-service dates, greatly simplifying recalibration and management of DeFelsko Inspection Instruments.
DeFelsko is pleased to announce the new Telescopic Probe Extender for PosiTector® 6000 Coating Thickness Gages. This lightweight, portable device increases the reach of PosiTector 6000 regular cabled probes up to 124 cm (49"), ergonomically measuring overhead or underfoot. Includes a built-in mount for securing the PosiTector gage body allowing for comfortable one-handed operation.
Features
DeFelsko is pleased to announce the new Bluetooth Printer, for wirelessly printing readings and statistical summaries from the shop floor or job site. This rechargeable, compact printer receives data from all PosiTector Advanced models - no gage update required. The new Bluetooth Printer is a direct replacement for the existing Martel printer, and will be included in all new printer orders.
Features
DeFelsko is pleased to announce the new Abrasives Test Kit for measuring the concentration of soluble salts in blast cleaning abrasives in accordance with ASTM D4940 and ISO 11127-6. The Abrasives Test Kit is ideal for use with the PosiTector SST Soluble Salt Tester and other conductivity meters.
To accommodate the new test kit, the measurement range of the PosiTector SST has been increased from 0 - 500 µS/cm to 0 - 1500 µS/cm. Existing probes can display measurements within the increased range after a gage update, but only probes shipped after March 12, 2018 are calibrated over the extended range, as reflected on the Certificate of Calibration.
Features
DeFelsko is pleased to announce the latest addition to the PosiTector DPM Dew Point Meter family. The PosiTector DPM IR includes the ambient temperature and humidity sensors from the PosiTector DPM Integral Probe plus an infrared surface temperature sensor. The infrared sensor doesn't require contact with the surface, making the inspection of large areas quick and easy. The 4:1 distance to spot ratio will average the temperature over a larger area making it ideal for quickly scanning large structures.
Features
DeFelsko is pleased to announce another new addition to the PosiTector 6000 series of coating thickness probes. The PosiTector 6000 F90ES probe features a 12 x 5mm (.048" x 0.2") probe head with 350mm (13.75") reach. It is ideal for measuring hard-to-reach areas and other challenging applications such as tight diameters, edges, and corners.
PosiTector 6000 F90ES Probe Specifications:
DeFelsko is pleased to introduce the new PosiTector® CMM IS Concrete Moisture Meter - In Situ probes for measuring relative humidity and temperature in concrete floor slabs. Collect measurements and generate reports in conformance with ASTM F2170, Standard Test Method for Determining Relative Humidity in Concrete Floor Slabs Using In Situ Probes. The PosiTector CMM IS probes are designed to wirelessly connect with the PosiTector App (iOS/Android) and PosiTector DPM Advanced models via Bluetooth. View the following video for an overview of this exciting new product.
Features
DeFelsko is pleased to announce two new kit options for the PosiTest® AT Pull-Off Adhesion Tester Series of instruments. The 50 mm2 Tile Kit conforms to BS EN 12004-2 and is ideal for measuring the tensile strength of ceramic tile cementitious, dispersion and reaction resin adhesives. The 50 mm C1583 Kit conforms to ASTM C1583 and is ideal for measuring the tensile strength of concrete surfaces, concrete repairs and overlay materials.The PosiTest AT Series measures the force to pull a specified test diameter of coatings or material away from its substrate using hydraulic pressure.
Features
The powerful new PosiTector® RTR 3D measures and records surface profile parameters using replica tape. Capture high-resolution 3D surface imagery and common 2D/3D parameters at a fraction of the cost of other instruments.
Features
DeFelsko is pleased to announce the availability of heavy-duty, waterproof Pelican cases for the PosiTest® AT Pull-Off Adhesion Testers and PosiTector® Inspection Kits. Each case comes complete with a custom foam insert to securely hold your PosiTest or PosiTector instrument. Pelican cases can be purchased as an upgrade from the standard case at the time of purchase, or as an accessory.
See more info on Pelican case for PosiTest AT: https://www.defelsko.com/accessories/atpelicancase
See more info on Pelican case for PosiTector Inspection Kits: https://www.defelsko.com/accessories/inspectionkitpelicancase
Testex Micrometer Kits include everything required to measure surface profile using replica tape
Features:
Notched Wet Film Thickness Gages measure the thickness of paint, enamels, and other wet films quickly and accurately
Features:
Determines a coating’s ability to resist separation from a substrate when a lattice pattern is cut into the coating in accordance with ISO 2409 and ASTM D3359
Features
Assesses the quantity and size of dust particles on blast cleaned surfaces in accordance with ISO 8502-3
Features
Determines the film hardness by pencil test (Wolff-Wilborn) in accordance with national and international standards including ISO 15184 and ASTM D3363
Features:
DeFelsko is pleased to announce the newest addition to the PosiTest line of pinhole and porosity detectors—the PosiTest HHD C High voltage Holiday Detector. The NEW compact, wand-style PosiTest HHD C uses continuous DC technology to detect holidays in coatings greater than 200 µm (8 mils) on metal and concrete substrates.
Features:
The new PosiTector GLS Gloss Meter brings Gloss, Reflectances, and Haze measurement to the PosiTector platform. Select up to three measurement angles to suit any application, save readings into memory, and transfer them to PosiSoft Software to quickly archive data and generate professional reports. The PosiTector GLS brings DeFelsko simplicity, durability, and accuracy to gloss measurement.
Features:
Featuring near-instant readings and no requirement to drill into the concrete, the PosiTest CMM is ideal for inspectors looking to quickly evaluate the moisture conditions in concrete slabs. It joins the DeFelsko line of concrete moisture measurement equipment alongside the highly-accurate PosiTector CMM IS In-situ Concrete Moisture Meter.
Features:
The new PosiTest HHD Basic Kit includes the same award-winning PosiTest HHD High voltage Holiday Detector in a more economical kit configuration. This new kit reduces weight and shipping costs while keeping the durability and versatility of the original, offering compatibility with all PosiTest HHD electrodes and accessories including the Handheld Wand.
New Features:
The PosiTest AT-M Manual Adhesion Tester has been updated with a new high-contrast, easy-to-read color display, a redesigned keypad, and field replaceable AAA alkaline batteries which provide up to 16 hours of testing. For easy setup and confirmation, the updated user interface shows important pull parameters before, during, and after the test.
New Features:
Featuring compatibility with all PosiTector probes manufactured since 2012, the new PosiTector gage body builds on this legacy with many industry leading new features.
New Features:
DeFelsko is pleased to announce the new PosiTest OTL Oven Temperature Logger. Featuring a high temperature stainless steel barrier box, the PosiTest OTL is ideal for measuring and recording oven temperature profiles during curing. Simultaneously measure up to 6 different temperatures at a time with a variety of air and surface temperature probes (sold separately).
Features:
Depending on time and temperature requirements, the PosiTest OTL is available in two configurations. The PosiTest OTL XT features an enhanced holder with heatsink for greater endurance at high temperatures.
A wide variety of temperature probes are available with 1.8 or 3.6 m (6' or 12') stainless steel braided cables (sold separately).
The new PosiTector DPM L Dew Point Meter Logger magnetically attaches to steel structures to measure and record climatic conditions at user-selected time intervals independently for up to 200 days. Stored datasets can be viewed or downloaded using a PosiTector Advanced gage body (S/N 784000+) or Apple/Android smart device.
At each interval, the PosiTector DPM L stores relative humidity, air temperature, surface temperature, dew point temperature, the difference between surface and dew point temperatures, and wet bulb temperature. Ideal for surface preparation as required by ISO 8502-4.
Features:
Introducing the new PosiTector 6000 FJS Coating Thickness probe for measuring thick, protective coatings on steel. With a measurement range of 0 to 25 mm (0 to 1.00 in.), It is ideal for measuring thick epoxies, rubbers, fireproofing, and other thick coatings applied to steel.
Compared to the higher range PosiTector 6000 FLS, this new probe features an alumina wear face and a lightweight, ergonomic design for comfortable all-day use. In fact, the new PosiTector 6000 FJS probe is about 66% smaller than comparable probes. Unlike competitive probes based on eddy-current technology, the electro-magnetic technology in PosiTector 6000 probes (including the PosiTector 6000 FJS) is less susceptible to the effects of substrate roughness, curvature, material, and alloy.
Introducing the PosiTector UTG CA, UTG CLF, and UTG P
DeFelsko is excited to announce a new probe for the PosiTector SPG Surface Profile Gage. The PosiTector SPG OS probe is ideal for measuring the peak-to-valley surface profile height of convex abrasive blast cleaned surfaces such as pipes and tanks.
Features
DeFelsko is excited to announce that the new PosiTest HHD High voltage Holiday Detector is now shipping. The PosiTest HHD uses pulse DC technology, offering a user-adjustable voltage range from 0.5 to 35kV for detecting holidays, pinholes and other discontinuities in coatings up to 20 mm (780 mils) thick.
The versatile PosiTest HHD is ideal for use with a wide range of rolling spring and flat wire brush electrodes — custom sizes are available upon request. Alternatively, use existing electrodes with industry-standard adaptors.
Key Features
The new PosiTest PC Powder Checker measures uncured powder coatings using non-contact ultrasound technology to predict a cured thickness. The instrument has been completely redesigned as a dedicated stand-alone unit -- no PosiTector gage body required. With a measurement speed up to 4x faster than previous models the new PosiTest PC is easier to use, especially on moving parts and challenging geometries.
Features
* Versus the previous generation PosiTector PC Powder Checker
The new PosiTector UTG CX Xtreme corrosion probe features the same trusted and precise ultrasonic technology as the PosiTector UTG Cprobe but with the addition of a robust braided stainless steel cable. It is the direct result of inspectors’ requests for a probe that features the same accuracy and ease-of-use of the current PosiTector UTG C but with the ruggedness to handle demanding applications.
Features
The new PosiTector BHI Barcol Hardness Impressor is DeFelsko’s latest addition to the PosiTector line of interchangeable probes. It is ideal for measuring the indentation hardness of soft metals (aluminum, aluminum alloys, copper, brass, etc.), harder plastics and fiber-reinforced plastics.
Features
The new PosiTector IRT non-contact Infrared Thermometer measures surface temperature from a distance - ideal for areas where conventional sensors will not work including hard to reach areas and moving parts. It is also ideal for measuring on objects too hot for direct contact sensors or when contact with a sensor would damage the surface.
Features
DeFelsko is pleased to announce the latest addition to the PosiTector DPM Dew Point Meter family. The PosiTector DPM IR includes the ambient temperature and humidity sensors from the PosiTector DPM Integral Probe plus an infrared surface temperature sensor. The infrared sensor doesn't require contact with the surface, making the inspection of large areas quick and easy. The 4:1 distance to spot ratio will average the temperature over a larger area making it ideal for quickly scanning large structures.
Features
DeFelsko is pleased to introduce the new PosiTector® CMM IS Concrete Moisture Meter - In Situ probes for measuring relative humidity and temperature in concrete floor slabs. Collect measurements and generate reports in conformance with ASTM F2170, Standard Test Method for Determining Relative Humidity in Concrete Floor Slabs Using In Situ Probes. The PosiTector CMM IS probes are designed to wirelessly connect with the PosiTector App (iOS/Android) and PosiTector DPM Advanced models via Bluetooth. View the following video for an overview of this exciting new product.
Features
DeFelsko is pleased to announce two new kit options for the PosiTest® AT Pull-Off Adhesion Tester Series of instruments. The 50 mm2 Tile Kit conforms to BS EN 12004-2 and is ideal for measuring the tensile strength of ceramic tile cementitious, dispersion and reaction resin adhesives. The 50 mm C1583 Kit conforms to ASTM C1583 and is ideal for measuring the tensile strength of concrete surfaces, concrete repairs and overlay materials.The PosiTest AT Series measures the force to pull a specified test diameter of coatings or material away from its substrate using hydraulic pressure.
Features
The powerful new PosiTector® RTR 3D measures and records surface profile parameters using replica tape. Capture high-resolution 3D surface imagery and common 2D/3D parameters at a fraction of the cost of other instruments.
Features